Temperature Effects on Magnetic Properties

Warm a paramagnet and watch its atomic magnets line up less and less as χ falls as 1/T, then heat iron past 1043 K and see its domains break up at the Curie temperature.

Interactive 3DPhysicsAdvanced7 min read

Drag to rotate · Right-drag to pan · Click, then scroll to zoom · Space play · Left arrowRight arrow step

What's happening

Formula & steps

    Your progress and quiz scores are saved on this device, and in your account once you sign up.

    Try this in the 3D model

    • In Warming a paramagnet, what happens to χ when the temperature doubles?
    • In Warming a paramagnet, why must T be in kelvin?
    • In The Curie temperature, what kind of material is iron above 1043 K?

    Heat stirs the atomic magnets

    Heat makes atoms jostle, and jostling atoms cannot line up their tiny magnets so well. So temperature changes how strongly a material is magnetised, in a different way for each kind of material.

    Paramagnets: Curie’s law

    In the 3D model, choose Warming a paramagnet and press Play. A paramagnet sits in a steady field.

    • At 50 K the jostling is small, so many atomic magnets lean along the field: χ is large.
    • Warm it, and they line up less and less.

    The susceptibility falls as 1/T. This is Curie’s law:

    χ=CT\chi = \frac{C}{T}

    where C is the Curie constant of the material and T is in kelvin. (Some books write it as χ=μ0C/T\chi = \mu_{0}C/T, with C defined a little differently; either way, χ goes as 1/T.) Here χ is 2.4×10−42.4 \times 10^{-4} at 300 K: doubling the temperature from 150 K to 300 K halves χ. Since M=χHM = \chi H and H=B0/μ0H = B_{0}/\mu_{0}, the magnetisation goes as B0/TB_{0}/T: a stronger field or a colder sample, more magnetisation.

    Ferromagnets: the Curie temperature

    Choose The Curie temperature. Inside one domain of iron at room temperature, the atomic magnets are all lined up by themselves. Heat it:

    • the domain’s magnetisation falls, slowly at first, then faster;
    • at 1043 K (770 °C), the Curie temperature TcT_{c}, the order breaks up completely. There are no more domains.

    Above TcT_{c} iron is only paramagnetic, with

    χ=CT−Tc\chi = \frac{C}{T - T_{c}}

    Cool it again, and the domains come back.

    material Curie temperature
    iron 1043 K (770 °C)
    nickel 631 K (358 °C)
    cobalt 1394 K (1121 °C)
    gadolinium 293 K (20 °C)

    Gadolinium is ferromagnetic only on a cool day.

    Diamagnets

    A diamagnet’s moments are made by the field itself, in each atom, so the jostling of heat hardly matters. Its χ stays almost the same at any temperature.

    Worked example

    A paramagnetic sample has a magnetisation of 12 A/m in a field of 0.5 T at 5 K. Find its magnetisation in a field of 0.25 T at 10 K.

    1. Curie’s law: M∝B0TM \propto \dfrac{B_{0}}{T}.
    2. M2=M1×B2B1×T1T2=12×0.250.5×510=M_{2} = M_{1} \times \dfrac{B_{2}}{B_{1}} \times \dfrac{T_{1}}{T_{2}} = 12 \times \dfrac{0.25}{0.5} \times \dfrac{5}{10} = 3 A/m.

    Remember: paramagnets obey Curie’s law, χ=C/T\chi = C/T with T in kelvin; a ferromagnet loses its domains at its Curie temperature and becomes paramagnetic, χ=C/(T−Tc)\chi = C/(T - T_{c}); diamagnets hardly change.

    Formulas and where to use them

    Curie’s law

    χ=CT,M=C B0μ0T\chi = \frac{C}{T}, \qquad M = C\,\frac{B_{0}}{\mu_{0}T}
    where
    CC
    Curie constant of the material (K)
    TT
    temperature (K)
    B0B_{0}
    applied field (T)

    Use it when: A paramagnet, not too cold and not too strong a field.

    Above the Curie temperature

    χ=CT−Tc,T>Tc\chi = \frac{C}{T - T_{c}}, \qquad T > T_{c}
    where
    TcT_{c}
    Curie temperature of the ferromagnet (K)

    Use it when: A ferromagnet heated above its Curie temperature, now paramagnetic.

    Common mistakes

    • Using degrees Celsius. Curie’s law needs the temperature in kelvin.
    • Thinking a hot magnet loses its magnetism gradually forever. Below Tc it weakens slowly; at Tc the domains vanish completely.
    • Applying Curie’s law to diamagnets. Their χ hardly changes with temperature.

    Quick check

    Test yourself — pick an answer to see if you got it.

    1. A paramagnet has χ = 2.4 × 10⁻⁴ at 300 K. At 200 K its χ is…

    2. Above its Curie temperature, a ferromagnet becomes…

    3. The Curie temperature of iron is about…

    4. The susceptibility of a diamagnet, when it is heated…

    5. A paramagnet has M = 12 A/m in 0.5 T at 5 K. In 0.25 T at 10 K its magnetisation is…

    Saved on this device.
    Spotted a mistake or a bug in the 3D model?

    Report a mistake

    in Temperature Effects on Magnetic Properties. Thank you — every report makes the lesson better for the next reader.

    We'll also include a link to the step of the 3D model you're on and your browser type, so we can reproduce it.